Gold Plating

MIL-DTL-45204, ASTM B488

Gold Plating is employed for their corrosion and tarnish resistance (including resistance to fretting corrosion and catalytic polymerization), bondability, low and stable contact resistance, solderability, and infrared reflectivity.

TYPES

Type 1 –  99.70%

Type 2 – 99.00%

Type 3 – 99.90%

GRADE

Grade A – Knoop Hardness 90 max

Grade B – Knoop Hardness 91 – 129,incl

Grade C – Knoop Hardness 130 – 200,incl

Grade D – Knoop Hardness 201 and over

CLASSES

Class 00 – minimum 0.508 µm  Class 3 – minimum 5.08 µm

Class 0 – minimum 0.762 µm   Class 4 – minimum 7.62 µm

Class 1 – minimum 1.27 µm   Class 5 – minimum 12.7 µm

Class 2 – minimum 2.54 µm   Class 6 – minimum 38.1 µm

GOLD PLATING-PROCESS CONTROL & TEST METHOD

VISUAL INSPECTION –  MIL-DTL-45204

HARDNESS  TEST – ASTM B578,ASTM E384

HEAT RESISTANCE TEST – MIL-DTL-45204

THICKNESS TEST – ASTM B486,2.ASTM B567,3.ASTM B568

SOLDERABILITY TEST – MIL-DTL-45204

ADHESION TEST – MIL-DTL-45204

HYDROGEN EMBRITTLEMENT MIL-DTL-45204

Comments are closed.